Overlaminating Film Troubleshooting Checklist
PROBLEM: Poor adhesion of the overlaminate to the print. CAUSES: Print not dry. Incompatibility of component parts. SOLUTIONS: In RIP phase use ink limiting setting to reduce ink deposit. Let ink dry for 24 hours, or longer…. Always follow the instructions of the ink & media manufacturers. Laminated prints should lay flat 24 hours before [ ]
http://bit.ly/2mQaDZG
Monday, March 6, 2017
See NEPATA Converting Equipment at ICE Expo Orlando
Supply55 will be exhibiting at the ICE Expo in Orlando April 25th, 26th and 27th, 2017 and will be featuring the NEPATA UA1650 ADWS converting center. Click the following link for a free pass to the show ICE EXPO FREE PASS. Click here to learn more about NEPATA Converting Equipment. Supply55, Inc. / NEPATA Converting [ ]