PROBLEM: Poor adhesion of the overlaminate to the print. CAUSES: Print not dry. Incompatibility of component parts. SOLUTIONS: In RIP phase use ink limiting setting to reduce ink deposit. Let ink dry for 24 hours, or longer…. Always follow the instructions of the ink & media manufacturers. Laminated prints should lay flat 24 hours before [ ]